[TheForge] Torch cutting tip

Washington, Aubrey O. awashington at ou.edu
Mon Jun 30 17:58:38 EDT 2008


You said you are using LP gas.  Are you ordering the correct tip for LP (rather than acet.)?

________________________________________
From: theforge-bounces at mailman.qth.net [theforge-bounces at mailman.qth.net] On Behalf Of Rich Maynard [rich at maynard.org.uk]
Sent: Monday, June 30, 2008 4:54 PM
To: 'Blacksmithing List Sponsored by ABANA'
Subject: RE: [TheForge] Torch cutting tip

I'm not sure, not really being an expert or even doingmuch flame cutting but
I get the feeling that using too big a nozzle might carry the heat away too
quickly - maybe because the gas flow is too high? I certainly find it easier
to cut 1/4 plate with the right size nozzle than with the one designed for
3"...

Rich M.

Richard Maynard - Artist Blacksmith
The Forge, Much Hadham, Hertfordshire SG10 6BS

The Forge Experience - be a blacksmith for a day!
http://www.muchhadhamforge.co.uk/experience.pdf

rich at muchhadhamforge.co.uk
www.muchhadhamforge.co.uk


-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Andrew Vida
Sent: 30 June 2008 22:46
To: Blacksmithing List Sponsored by ABANA
Subject: Re: [TheForge] Torch cutting tip


Lynn -

There is no reason you cannot burn sheet metal with a larger tip.  The
only reasons I can think of to use a smaller tip are:

        - lower fuel consumption
        - smaller kerf
        - smaller heat effected zone

These may be very valid reasons for using the smaller tip, but if you're
not cutting lots of sheet and if kerf dimension is not critical, then I
see no reason not to have to go to the smaller tip.  I can remember
watching Parker Bohn very expertly burn some galvanized corrugated sheet
with his normal large-sized torch.  No problems.  Of course, he was a
super expert welder/cutter. :)

Lynn and Susan Lang wrote:
> Hello
> I am having trouble with my local gas supplier ordering the correct
> tip for my cutting head, they order and when it gets here it does not
> fit.....The reason for ordering a smaller tip is to cut sheet metal as
> suggested by the owners manual. Do I need a smaller tip to cut sheet
> metal or do I learn how to use the size 1 tip to cut the sheet metal?
>
> The torch (Victor) came supplied with a series 3 size 1 tip, I have
> ordered the 000 size, and I am using LP gas.
>
> Thank you
> lynn
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
>
>

--

        -Andy V.

no .sig
go .fig
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________


No virus found in this incoming message.
Checked by AVG.
Version: 8.0.101 / Virus Database: 270.4.3/1526 - Release Date: 6/30/2008
8:43 AM

_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________


More information about the TheForge mailing list