[TheForge] bad thread -ersatz and back to thread

Jim Beard regionalchaos at gmail.com
Wed Jun 11 13:04:32 EDT 2008


There was a thread over on iForgeIron a while back about a fellow that
set up a waste oil forge.  He was slowly dripping oil into a forced
air burner.  I'll see if I can dig up the link...

http://www.iforgeiron.com/forum/f7/waste-oil-burning-forge-4219/

It looked pretty interesting to say the least.

Jim
Eugene, OR

On Wed, Jun 11, 2008 at 8:47 AM, lee robbins <naturadoc1 at yahoo.com> wrote:

>
> About 7 dollar kerosene at lowes?  Get a gas can and
> you can drop it to a cheap 5 dollars a gallon, even
> less if you get it for home heating and avoid the
> taxes. When i was in Kumamoto, japan at Mitsu's
> (takamitsu toshinobu) studio, he has taught at
> Campbell Folk, he forged iron using kerosene. no forge
> welding though. In the '90's it was a cheaper
> alternative to propane.
>
> Lee
>
>
>
>
>
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
>
>
>


More information about the TheForge mailing list