Tig uses CC (constant current) same as stick welding. Tig Polarities: Steel - DCEN (EN - electrode negative, ground positive) Stainless - DCEN Alum - AC (requires high frequency) Mig uses CV (constant voltage) so you can't use a mig for a tig.