James,
Please send them to me. Thanks.
Bob
_____
On Jun 2, 2008, at 7:20 AM, Cindy and James wrote:
> I found a pamphlet from Sears, of all places, when cleaning out an old
> file cabinet... has a diagram and instructions on how to set up a TIG
> using a plain DC welder. If I can figure out how to post the pictures
> (2), I will, or if anyone wants to see it I can email them directly.
> The pamphlet must be at least 35 years old, maybe more, could not find
> a date.
>
> James Allcorn
>>
>> Bob,
>>
>> All you need is a DC power source. I disagree with another post as to
>> how a manual torch (valve to let gas thru on the torch head) is a
>> PITA. It's like turning water on and off . Sure, you will damage
>> your tungsten if you light up without gas. I use this setup
>> exclusively and do a lot of tig welding . I'm a pretty good welder
>> and still have to sharpen plenty of tungsten.You don't need a foot
>> pedal to regulate amperage, just set your heat at the machine and
>> adjust up or down based on what you are welding (different
>> thicknesses, materials etc) Tig is welded with strait polarity so the
>> ground is positive, torch negative. Argon gas, approx.20lb pressure
>> on your regulator. Piece of cake. I learned how to tig weld building
>> and repairing boilers in the field. We didn't weld with pedals etc.
>> On a big job we were lucky if they had remote rheostats to change our
>> heat without running to our machine and back if we were switching
>> from tig to stick etc. I believe there is a mystique about tig
>> welding, that it's specialized so it's harder than other forms of
>> welding. Like anything else you want master, it just takes time and
>> practice.
>>
>> Bill Woolley
>>
>>
>>
>>
>>
>>
>>
>> schade at acegroup.cc wrote:
>>> I think I remember reading here some time ago about a way to turn an
>>> arc welder into a scratch start TIG welder.
>>>
>>> Am I dreaming or is this doable? If it is can someone point me in
>>> the right direction?
>>>
>>> Thanks.
>> 9.24.4/1476 - Release Date: 5/31/2008 12:25 PM
>>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
More information about the TheForge
mailing list