[TheForge] Re: Free the Stake!

Tod Estes testes at medicine.nodak.edu
Mon Jan 21 23:00:41 EST 2008


How about cooling the large block with a mix of acetone and dry ice, heat the
stake with a non-flame heat source. and tap to see if one or another moves. I
guess you could use just liquid nitrogen and then try to heat the stake. Not as
much fun as explosives.
Quoting Andrew Vida <osan at netlabs.net>:

>
>
> Larry Brown wrote:
> >
> > Something I haven't seen suggested:
> > Cut the stake off close to the block. Reforge a taper on the stake.
> > Drill a bunch of holes in the stub making as large a hole as possible or
> > blow through with a torch. Heat the stub remains with a torch,
> > preferably a large or rosebud tip. This will force the stub to upset
> > into itself and will probably fall out or be easily driven out after
> > cooling with the block upside down
>
> 	That would have to be a hell of a jam to warrant that much surgery.
>
> 	How about dynamite?  No, probably would not do the job, but the great
> big <kaboom> would be fun.
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
>
>
>


Tod Estes

People do not care about how much you know
until they know about how much you care.


More information about the TheForge mailing list