[TheForge] Sucker rod
xlch58 at swbell.net
xlch58 at swbell.net
Fri Jan 18 23:13:38 EST 2008
Woolley wrote:
> I have never heard the term "sucker rod " before. Where does it come
> from?
>
>
>
>
Must not be from Texas. We had several corrals built from well casing
for posts and sucker rod for rails. Sucker rod is used to connect the
oil well pumping machinery on the surface(Walking beam, or donkey as we
called them) with the plunger at the bottom of the well. It comes in 25
foot lengths and has a alternating male and female threads at each
end. It is screwed together to make up the required distance between
the top of the well and the bottom.
Charles