I have never heard the term "sucker rod " before. Where does it come from?
David E. Smucker wrote:
> Bob, It been more than 40 years since I was a young engineer working
> in the oil patch but back then we had a series of different alloys to
> use in different wells depending on the type of corrosion problem we
> might have in a given well producing from a given formation. In fact
> we had a series of very short sucker rods -- we call them pony rods --
> about 2 foot in length that we could put down a well to test which
> type of rod gave the best life under real world conditions.
>
> All of that said, our most common rod material was 4140 or 4340 or
> some similar alloy. My starting point in making tooling from sucker
> rod would be to assume that it is 4140 and make a test piece. Both
> 4140 and 4340 are oil quenching. I happen to have some 7/8 dia 4340
> that I obtained through a local scrap dealer and it makes great
> tooling, tongs etc. You should have good luck with your sucker rod.
> Oil companies pay good money to have high performance out of sucker
> rods. It gets expensive to have to do down hole repair work because
> you have failed sucker rods.
>
> Dave Smucker
> ----- Original Message ----- From: "Bob Ehrenberger"
> <eforge at centurytel.net>
> To: "theforge" <theforge at mailman.qth.net>
> Sent: Friday, January 18, 2008 9:48 AM
> Subject: [TheForge] Sucker rod
>
>
>> I picked up some sucker rod last week and was told that it was good for
>> making hand tools. Do any of you know what steel it is? or the
>> composition
>> of alloys in it?
>>
>> Robert Ehrenberger
>> Shelbyville, Mo.
>> eforge at centurytel.net
>>
>>
>>
>> _______________________________________________
>> Manage membership or unsubscribe at:
>> http://mailman.qth.net/mailman/listinfo/theforge
>> theforge mail list group photo site is
>> http://www.photoaccess.com
>> Login: blacksmithblacksmith at hotmail.com
>> password: anvil
>> ___________
>>
>>
>>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
>
More information about the TheForge
mailing list