Already got a jar ready!
On Jan 1, 2008 11:51 AM, Andrew Vida <osan at netlabs.net> wrote:
>
>
> Daniel Kretchmar wrote:
> > Thanks Andy! I notived my dragons breath forge was getting as hot as
> > it should yesterday and when I pulled the bricks away from the
> > openning, I noticed a gap between the poured refractory and the
> > kaowool. The gap was white hot! I turned off the forge and I'll
> > replace the kaowool today. I worked with coal and charcoal for a bit
> > and refined the wrought a bit more, but I wanted wait for the gas for
> > before welding. My welding in the coal forge tends to leave
> > inclusions. No problem when making axehead, but not good when making
> > a knife for the wife! I am going out to work in the shop for most of
> > the day......HAPPY NEW YEAR!
>
> You're welcome. If you have not used it yet, I would strongly
> recommend you coat the inside of the new wool with either satanite or
> ITC-100. These reflective coatings make a BIG difference in how the
> forge operates. You can either attain higher temperatures or use
> significantly less fuel.
>
> -andy
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
More information about the TheForge
mailing list