[TheForge] fire screen
Andrew Vida
osan at netlabs.net
Thu Feb 28 14:56:27 EST 2008
Wow.. really? That seems a mite meaty. I was think 14 to 18.
Huh...
dan tull wrote:
> 10ga. X .035
> McNicols
>
> ----- Original Message ----- From: "Andy Gladish" <gladish at cablerocket.com>
> To: "Sponsored by ABANA" <theforge at mailman.qth.net>
> Sent: Thursday, February 28, 2008 9:56 AM
> Subject: [TheForge] fire screen
>
>
>> Could someone please recommend a wire size for the screen on a
>> freestanding fire screen?
>> I spent some time on McMaster's website but with 98948.9834 X 10^7
>> choices
>> it just gave me a headache...
>> Thanks!
>>
>> Andy Gladish
>> _______________________________________________
>> Manage membership or unsubscribe at:
>> http://mailman.qth.net/mailman/listinfo/theforge
>> theforge mail list group photo site is
>> http://www.photoaccess.com
>> Login: blacksmithblacksmith at hotmail.com
>> password: anvil
>> ___________
>>
>>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
--
-Andy V.
no .sig
go .fig
More information about the TheForge
mailing list