[TheForge] Gas forge pic (Re: News for a slow day)
Mike Spencer
mspencer at tallships.ca
Tue Dec 30 12:49:45 EST 2008
Weeks ago, Bruce wrote:
> Post some pictures! Please. I'd like to see your design.
and I said I'd post one RSN. I just realized that I took the pic but,
as far as I can tell (or remember) I didn't make it accessible to the
net.
So look here:
http://home.tallships.ca/mspencer/temp/gas-forge.jpg
I've had it running. From the perspective of someone who has minimal
experience with anything but coal, it works fine, heats well and
quickly with ca. 5 PSI. I use refractory brick for "doors" as
needed.
- Mike
--
Michael Spencer Nova Scotia, Canada .~.
/V\
mspencer at tallships.ca /( )\
http://home.tallships.ca/mspencer/ ^^-^^