Peter Hirst wrote:
> Well, if you say that because wrought iron is inherently non-modern, I 
> would have to agree.  But if you mean its not being made any more, it 
> is.  One firm in England is still producing it.

	All they do is rework wrought iron scrap into useful material.  To my 
knowledge, nobody on the planet is still producing new wrought iron.