[TheForge] Re: Flux

Franklin Police 780 at mchsi.com
Tue Apr 15 16:07:38 EDT 2008


That pesky Bad Roger he is always selling people those DVDs
That one was RD70 with Mark Pearce at Bemidji, MN.  He lives in Canada now.
I saw him last at the Seattle ABANA conference
List of videos is at www.umbaonline.org
$5 each

I plan to have them with at BAM 08 so if you are going there bring your list
of the ones you want.
I have been working on my ring to submit to the contest.  The ring is steel
the rest copper

Roger R Degner



-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of robert hensarling
I have a DVD that Roger sold me showing a English guy demonstrating here in 
the States.  He did several forge welds using no flux at all.  He was very, 
very fast from the forge, to the tap, tap, tap, hammer, hammer.  I was 
impressed and ran to the shop to try it.  Need I say more?