[TheForge] flux
Lynn Emrich
theatre_weapons at yahoo.com
Tue Apr 15 09:44:58 EDT 2008
Is that the same thing that I get in the bucket under my grinder?
Lynn
----- Original Message ----
From: kim george <klgeorge at kent.edu>
To: theforge at mailman.qth.net
Sent: Tuesday, April 15, 2008 9:33:31 AM
Subject: [TheForge] flux
I add iron-steel to my borax. I get it by going to a garage that turns
drums and rotors. They give it away. It's also good for helping roses bloom.
Kim George