Yes, welding inside with little or no breeze.

________________________________________
From: theforge-bounces at mailman.qth.net [theforge-bounces at mailman.qth.net] On Behalf Of Todd Rich [torin at panix.com]
Sent: Thursday, October 11, 2007 1:13 PM
To: Sponsored by ABANA
Subject: RE: [TheForge] MIG Question

On Thu, 11 Oct 2007, Washington, Aubrey O. wrote:

> Thanks Tod(d).  (Both of you.)
>
Hope it was useful.  Btw, I'm assuming you are welding inside and that
there isn't a lot of wind.  I've had the garage door open on my shop and
had a breeze mess up a weld by blowing away the shielding gas before.
                Todd (the 2 d one...gee that sounds like a droid...)