On Thu, 11 Oct 2007, Washington, Aubrey O. wrote:

> Thanks Tod(d).  (Both of you.)
>
Hope it was useful.  Btw, I'm assuming you are welding inside and that 
there isn't a lot of wind.  I've had the garage door open on my shop and 
had a breeze mess up a weld by blowing away the shielding gas before.
 		Todd (the 2 d one...gee that sounds like a droid...)