[TheForge] RE: Chop Saw; carbide blade

Washington, Aubrey O. awashington at ou.edu
Tue Nov 13 15:53:10 EST 2007


Thanks.  So far I don't use the chop saw enough to invest in the expensive carbide blades.  But, someday I may consider it.  I hate the noise and mess of a chop saw, but it's the quickest way to do some jobs.

Aubrey

________________________________________
From: theforge-bounces at mailman.qth.net [theforge-bounces at mailman.qth.net] On Behalf Of Ron Childers [munlaw2 at hcsmail.com]
Sent: Tuesday, November 13, 2007 1:00 PM
To: 'Sponsored by ABANA'
Subject: [TheForge] RE: Chop Saw; carbide blade

Aubrey,

I think you can use a carbide on any heavy duty chop saw if it is the
correct size. Wiregrass Forge is replacing the abrasive blade with a carbide
blade. Don't cut stainless with a blade made for mild steel- it will dull
it.

Ron C

-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Washington, Aubrey O.
Sent: Tuesday, November 13, 2007 11:49 AM
To: Sponsored by ABANA
Subject: Chop Saw [ Was: RE: [TheForge] art as art]

Lee,

Can you put a carbide blade in any chop saw?  Or do you need a special saw
to use the blade?

Aubrey

________________________________________
From: theforge-bounces at mailman.qth.net [theforge-bounces at mailman.qth.net] On
Behalf Of lee robbins [naturadoc1 at yahoo.com]

I used my new carbide chop saw for the first time
today. Wow, almost no noise, no flying debris or
sparks. Amazing. I had no idea. plus a narrow clean
kerf. Im a slow learner.

Lee
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________




_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________


More information about the TheForge mailing list