I think you can use a carbide on any heavy duty chop saw if it is the
correct size. Wiregrass Forge is replacing the abrasive blade with a carbide
blade. Don't cut stainless with a blade made for mild steel- it will dull
it.
Ron C
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Washington, Aubrey O.
Sent: Tuesday, November 13, 2007 11:49 AM
To: Sponsored by ABANA
Subject: Chop Saw [ Was: RE: [TheForge] art as art]
Lee,
Can you put a carbide blade in any chop saw? Or do you need a special saw
to use the blade?
Aubrey
________________________________________
From: theforge-bounces at mailman.qth.net [theforge-bounces at mailman.qth.net] On
Behalf Of lee robbins [naturadoc1 at yahoo.com]
I used my new carbide chop saw for the first time
today. Wow, almost no noise, no flying debris or
sparks. Amazing. I had no idea. plus a narrow clean
kerf. Im a slow learner.
Lee
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge
mailing list