[TheForge] MIG Welders
Lon Humphrey
ironcrossforge at roadrunner.com
Tue May 22 12:57:56 EDT 2007
ive had less trouble with the feeding of wire with the millers stanless,
carbon steel dosent seem to matter it eats both well...
and for me thats a biggie really pisses ya off when you have to stop to
screw with the liner or feed rolls
i used a lincoln that just would not feed stainless had a sales rep in to
look at it and he said that the gun had been bent .......he left the shop
quickly
just my experiance........ lincoln freed the slaves but he didnt build
welders
----- Original Message -----
From: "Washington, Aubrey O." <awashington at ou.edu>
To: "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Tuesday, May 22, 2007 12:16 PM
Subject: RE: [TheForge] MIG Welders
Okay, Lon, I'm listening. I'm in a position to buy either a Lincoln MIG
140C or a Millermatic 140. Tell me why you like Lincolns better than
Millers. Give me some data I can use to help me make the choice.
Aubrey
________________________________
From: theforge-bounces at mailman.qth.net on behalf of Lon Humphrey
Sent: Tue 5/22/2007 10:25 AM
To: Sponsored by ABANA
Subject: Re: [TheForge] MIG Welders
i would not be afraid to try this with 250 amp mig welder even a junk
lincoln one ...IMHO i like miller but i know guys that hate millers and the
only hobart welder ive ever used is a portable stick welder and its too
small
just bevel your edges make sure its clean and go like hell
you said +" So Lon, should I get the 251 or the 210? " not sure what your
talking about ... i missed half the thread most i dont read but i caught the
part about gasses and plate thickness
----- Original Message -----
From: "Todd Rich" <torin at panix.com>
To: "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Tuesday, May 22, 2007 10:52 AM
Subject: Re: [TheForge] MIG Welders
>
>
> On Tue, 22 May 2007, Lon Humphrey wrote:
>
>> 3 inch fillit xray on a large pressure vessel ----- Original
>> Message ----- From: "Mark A. Pesetsky" <pesetsky at Princeton.EDU>
>> To: "Sponsored by ABANA" <theforge at mailman.qth.net>
>> Sent: Tuesday, May 22, 2007 10:27 AM
>> Subject: RE: [TheForge] MIG Welders
>>
>>
>> How thick a weld have you done?
>>
>> Thanks
>> Mark
>
> Mark, if Lon says anything that contradicts me on MIG welding, I'd go with
> what he says. He is way out of my league :).
>
> So Lon, should I get the 251 or the 210? I'm doing a large Kinyon, plus
> I've got some other projects that could use a decently large machine.
> Including some potential copper welding jobs.
>
> (Sorry if you have already commented on it, I'm not archiving mail from
> this list, and I'm lousy with names.)
>
> I do have a stick welder that will eventually be coming home, but my welds
> with it always look like they were done by a drunken baboon. I can't even
> weld up a quench tank with it that doesn't leak. With the the WP 100 it
> took me 10 minutes (mainly waiting on the duty cycle) and didn't leak and
> looked nice on top of that.
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com <http://www.photoaccess.com/>
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com <http://www.photoaccess.com/>
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
--------------------------------------------------------------------------------
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
More information about the TheForge
mailing list