[TheForge] MIG Welders

Mark A. Pesetsky pesetsky at Princeton.EDU
Tue May 22 09:54:30 EDT 2007


1/2" plate is the thickest welds that I will have. Not going to buy a
stick welder just for this. Will do multiple passes I guess....But the
gas addition was needed I know that and have been meaning to do it, just
didn't have the need like I do now. Just a matter of getting aquainted
with the new set up...

Thanks
Mark 



half inch plate?? multiple pass with a gas mixed with a smaill about of
oxygen so you can spray it on ....OR stick weld it



More information about the TheForge mailing list