I have also used Permalac outdoors with some success. I wouldn't apply
over wax, paint is_ probably _ok depending of course on how well the
paint was applied. Go to Peacock's website for pretty extensive
how-to. The link was in another message. I have found that I have to be
very careful about complete coverage when applying this product. I
usually brush it on. They carry two different thinners of which I use
the one that evaporates at a slower rate after having some trouble with
the other. Also as with any clear or paint for that matter, the finish
is only as good as the prep. Make sure you remove all your rust or the
finish will breakdown over time.
Regards,
Bill Woolley
Hufford, David wrote:
> Can Permalac be applied over a wax or oil finish, such as beeswax or
> dried linseed oil? How about over paint? Or does it only adhere to
> bare metal?
> David Hufford
> Richmond KY
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
>
>
More information about the TheForge
mailing list