Tyanks for the info, lets see I have a bead blaster
for rough cleaning, a good little shop vaccum for
final cleaning and a fair size oven for the final
baking.
Many thanks,
Jerry
--- Dan Brewer <danqualman at gmail.com> wrote:
> The instructions that come with the harbor freight
> are good. Big thing is
> keep the work area and the work clean. Set up a
> spray booth. It doesn't have
> to be much. Just an area that you spray in that you
> can vacuum up after you
> are done. Look here
> http://en.wikipedia.org/wiki/Powder_coating
> Having an area that has a positive air flow away
> from you and through some
> type of filter to capture the residual powder and a
> place to hang your
> parts.
> Here is a home made gun
>
http://www.flickr.com/photos/zapwizard/145361494/in/photostream
>
>
>
> Dan in Auburn
>
>
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net
> [mailto:theforge-bounces at mailman.qth.net] On Behalf
> Of Jerry Smith
> Sent: Sunday, March 18, 2007 11:29 AM
> To: The Forge
> Subject: [TheForge] OT sort of Powder Coating
>
> Folks,
>
> Do we have any one out there who does powder
> coating?
> I wan to learn how to do it, and also how to avoid
> the
> mistakes.
>
> I don't have the gun or the basic kit, but I do have
> a
> compressor and a good size oven.
>
> Jerry
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
More information about the TheForge
mailing list