What about RG45 tig rod it is basically 1008
Jim
On Mar 12, 2007, at 11:35 PM, Peter Fels And Phoebe Palmer wrote:
> Been frustrated trying to forge torch welded parts and sheet.
> The available rods have alloying elements designed to work as
> deposited...not forged, reheated, rewelded, hammered cold and hot
> and so on.
> So i thought...would pure iron welding rod work?
> If so, where can i get some?
> AK steel no longer lists it apparently....pete f