[TheForge] pure iron wire?
Peter Fels And Phoebe Palmer
artgawk at thegrid.net
Tue Mar 13 01:35:15 EST 2007
Been frustrated trying to forge torch welded parts and sheet.
The available rods have alloying elements designed to work as
deposited...not forged, reheated, rewelded, hammered cold and hot
and so on.
So i thought...would pure iron welding rod work?
If so, where can i get some?
AK steel no longer lists it apparently....pete f