[TheForge] Miniature air-arc
Kathy
keporter at comcast.net
Sun Jun 24 19:16:40 EDT 2007
You're welcome, Larry.
Once you boys have built your toys,
and are grinning about all they can do,
"the others will soon be wanting one too"
:-)
I've learned to be patient about how long good ideas take to catch on. It seems
to have something to do with the rise of inertia doubling in direct proportion
to the actual value of the notion, or something like that :)
Mikey
-----Original Message-----
From: theforge-bounces at mailman.qth.net [mailto:theforge-bounces at mailman.qth.net]
On Behalf Of Larry Brown
Sent: Sunday, June 24, 2007 3:36 AM
To: Sponsored by ABANA
Subject: RE: [TheForge] Miniature air-arc
Thanks for the info, I want to play around with this a bit
Larry Brown
At 11:18 AM 6/23/2007 -0700, you wrote:
>To L Brown,
>Yes, but it's a minor item that will be thrown in for thoroughness; also, it
>wasn't an invention of my own. Therefore, I don't mind blabbing on the net
>about
>how to build one, but on the other hand will not go to the trouble of
>providing
>a drawing until I construct the equipment for the chapter on air gouging
>in the
>book. Furthermore, I haven't built a miniature air-arc torch in thirty-five
>years, so my memories may be less than letter perfect; for instance, I
>remember
>the DC current used as about 65 amps and the air pressure as 45 PSI, but your
>results may vary. Don't use too much air pressure, as the vibration it creates
>will snap your carbons off (see needle valve advice further on).
<Big Snip>
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge
mailing list