[TheForge] oxy-propylene

Chris Caswell olayers at sover.net
Fri Jun 22 20:15:53 EDT 2007


I was wrong - the set will run propylene or propane - I bought it today 
and cut through 1" square as fast as I could move the torch.  I have not 
done any heating with it yet.

Chris Caswell
Caswell Wood & Iron
24 1/2 Pomeroy Street
Burlington, VT 05401





Jerry Frost wrote:
> I know little to nothing about propylene as a fuel but even if it has 
> better heating properties is it easy to get? I mean commonly available 
> at every second gas station, Home Depot, 7-11, etc.? Is it economical? 
> Say around $12.00 for a 20lb. / 5gl. bottle?
>
> I know I see propane signs and tanks everywhere; you can get a tank 
> filled even in the remotest parts of Alaska. I don't recall ever 
> seeing propylene for sale, at least not advertised. So, where would I 
> look for it? What would I expect to pay for the equivalent of 20lbs of 
> propane?
>
> The downside to an All-States oxy propane rig is it's initial price. 
> Last time I checked they were running around $650 for the set. If you 
> want the special propane tank that fits your oxy acet cart that's 
> extra. The upside is that by the time I'd used up my first 20lb. 
> bottle of propane it'd paid for itself about 3 times over. Consumables 
> for the All-States oxy propane rig are about 2% what oxy acet is for 
> the same amount of work.
>
> Is propylene that much better?
>
> Frosty
> -------------------------------
> If it ain't forged
> it ain't real.
> Wrought iron is.
> The FrostWorks
>
> Meadow Lakes, AK.
>
> http://www.artmetalradio.com/
>
> From: "Chris Caswell" <olayers at sover.net>
>
>> I would be getting a set designed specifically for oxy-propylene - 
>> not a super heavy duty one but as I prefer to use the coal forge as 
>> my primary heat source I think that will be ok!
>>
>> -- 
>> Chris Caswell
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
>
>
>


-- 




More information about the TheForge mailing list