> If you're working long enough sections to use the pipe as a handle (until you cut to length), remember to plug the handle end of the pipe with a wet rag or something.  Hot gas will travel up the pipe like a chimney.  Also, be very careful if you quench hot pipe; steam and hot water can shoot up the pipe and out the handle end.
>
> If you're working short sections with tongs, then you don't have to worry with this stuff.
>