That may be true, but seamless tubing is made by a technique that amounts to being drawing out in the round.

For non-structural work, it probably makes no difference.

Bruce
NJ

>>> damales at Pollybutte.net 6/18/2007 1:18:36 AM >>>
When I worked my first piece of wrought Iron. I found out real quick that if
you don't go square, octagon then round as you draw you end up with a torn
up mess. With mild steel it really is very forgiving. And you can draw from
any shape.
Dan Scheid

-----Original Message-----
From: theforge-bounces at mailman.qth.net 
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Bruce Freeman
Sent: Sunday, June 17, 2007 9:02 AM
To: Sponsored by ABANA
Subject: Re: [TheForge] Project advice

Bob,
I'm not sure we're communicating.
I was taught, and I teach, that you take any bar to
square (though hex works too) and forge it as far as
necessary.  If you want it round, you THEN go to
octagonal then round.  That's what I mean by SOR.
Bruce

--- schade at acegroup.cc wrote:

> 
> On Jun 17, 2007, at 7:56 AM, Bruce Freeman wrote:
> >  (noting that 'SOR'
> > does NOT apply to pipe),
> 
> 
> I never "SOR" anyway. I just go straight to "S" and
> draw away. I think 
> "SOR" might have some good reasons if forging 3"
> stock but for forging 
> 3/4" and down to a smaller size "SOR" seems a waste
> of time. BTW I am 
> using a powerhammer.
> 
> Bob
> 
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge 
> theforge mail list group photo site is
> http://www.photoaccess.com 
> Login:  blacksmithblacksmith at hotmail.com 
> password:  anvil
> ___________
> 
> 
> 




 
____________________________________________________________________________
________
Need Mail bonding?
Go to the Yahoo! Mail Q&A for great tips from Yahoo! Answers users.
http://answers.yahoo.com/dir/?link=list&sid=396546091 
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge 
theforge mail list group photo site is
http://www.photoaccess.com 
Login:  blacksmithblacksmith at hotmail.com 
password:  anvil
___________


_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge 
theforge mail list group photo site is
http://www.photoaccess.com 
Login:  blacksmithblacksmith at hotmail.com 
password:  anvil
___________





More information about the TheForge mailing list