[TheForge] Argon-CO2 mix question
Larry Brown
lp.brown at verizon.net
Tue Jun 5 21:16:47 EDT 2007
Never heard of them separating and after many years of using Argon- CO2
(C-25) I have never had the gas act differently while welding which would
indicate separating. I have a tank that had a sticker about an eductor tube
when I got it but I have been hearing it rolling around inside it for years
- No difference when it was attached or loose.
A real man would grab that sucker and shake it like a can of paint! (Please
leave the cap on)
;-)
Larry Brown
>If you're really concerned, lay your cylinder on it's side and roll it
>back and forth across the floor a couple times. Disconnect the regs and
>put the cap on first. (I hope I didn't have to say that but better safe
>than sorry)
>
>Frosty
>-------------------------------
>If it ain't forged
>it ain't real.
>Wrought iron is.
>The FrostWorks
>
>Meadow Lakes, AK.
>
>http://www.artmetalradio.com/
More information about the TheForge