Good point Andy. I don't know if the modern bladder 
pressure tanks are galvy but it makes sense they would 
be.

I don't recommend anyone expose themselves to zinc 
smoke unnecessarily but it isn't the danger it's 
reputation claims. There are also safe ways to remove 
the galvy like a vinegar soak.

Still, galvy's another point in favor of something else 
for a forge shell.

Frosty
-------------------------------
If it ain't forged
it ain't real.
Wrought iron is.
The FrostWorks

Meadow Lakes, AK.

http://www.artmetalradio.com/

From: "Andy Gladish" <gladish at cablerocket.com>


>
> I would want to make sure that the vessel I use for a 
> forge shell is not
> galvanized, IE zinc coated.
> Believe all the well tanks are- the fumes are awful 
> when they get hot.
>
> Andy G.
>
> 