Salt water will work and let it sit outside for a bit. Looks nice
under a clear coat spray.
Rob
On Jul 12, 2007, at 19:03, Wayne Ackman wrote:
I have a job where he wants a rust finish. I tried muriatic acid, and
some stuff I bought called Easy Rust Finish. Not so easy really, you
have to remove every bit of the mill scale. both did a rust finish but
it is an orange color. He wants it to be more reddish than I am
getting. I heard ferric nitrate might do the trick. Opinions? Also
where would I get that? Besides ordering it online, i mean. thanks
for any suggestions
Wayne