Jerry> ...an old truck spring for the actual drag bar.
Frosty> No problem forging 5160 Jerry...
I don't know about 5610 but I forged a replacement tine for my
Troy-Built tiller from new truck spring -- offcut from the spring shop
-- and it's on its 3rd year and doing fine.
- Mike
--
Michael Spencer Nova Scotia, Canada .~.