--- Bruce Freeman <freemab222 at yahoo.com> wrote:
> With SS, you don't need it anywhere near this thick,
> which is good because SS is expensive.
>
> I suggest 14 to 16 gauge, with stiffeners beneath,
> especially around the firepot. This surface should
> never get particularly hot.
>
> I haven't seen you discuss the hood. Even outdoors
> you want a side-draft hood and enough flue pipe to
> carry the smoke to well overhead.
>
> Bruce
> NJ
>
> --- Jerry Smith
> <jerry_smith at anvilsandinkstudios.com>
> wrote:
>
> > What type of stainless steel, I would say 1/4 for
> > the
> > bottom plate and something like 10 guage for the
> > sides.
> >
> > I have a small MIG welding for the tack welding
> and
> > a
> > Tomnstone to do the seam around for the sides.
> What
> > electrodes for the side seams 308/308L, 309/309L
> or
> > 316/316L
> >
> > Am I on the right track for making this from
> > stainless?
> >
> > I figure the legs I can use black iron pipe, and
> > find
> > some wheels to make the movable.
> >
> > Jerry
> >
> >
> > _______________________________________________
> > Manage membership or unsubscribe at:
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://www.photoaccess.com
> > Login: blacksmithblacksmith at hotmail.com
> > password: anvil
> > ___________
> >
> >
> >
>
>
>
>
>
____________________________________________________________________________________
> Yahoo! oneSearch: Finally, mobile search
> that gives answers, not web links.
>
http://mobile.yahoo.com/mobileweb/onesearch?refer=1ONXIC
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
More information about the TheForge
mailing list