	I use a band saw to cut the blank instead of trying to hot chisel
the piece apart. I have not been able to get the chisel to meet exactly in
the center of the bar reliably and a real mess that cannot be corrected is
the result. The secret to the diamond shaped hole is overlapped cuts 90
degrees apart along the axis of the bar stock. If you are using 1 inch
square bar the overlap is 1 inch - or equal to the parent stock cross
section. On 1/2" sq overlap the cuts 1/2". The only other decision is how
long do you want the arms and the top and bottom piece to be. It is easier
to do than to describe. 


Bob Willman
Bowling Green, Ohio
The Eagle's Anvil
WB8NQW

-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Fiorini & Skiles
Sent: Tuesday, January 02, 2007 9:56 PM
To: theforge at mailman.qth.net
Subject: [TheForge] forged cross

Is there an on-line tutorial for how to make a christopher cross?  I think I
have the name right...  If not, does anyone know which book it is shown in?

Someone once gave me a lovely bronze christopher cross.  I'm thinking it
would be a nice fundraiser item for our church.
-Kirsten
www.knitsteel.blogspot.com 

_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________







More information about the TheForge mailing list