[TheForge] Traveling Gas
Steve Smith
sos at alum.mit.edu
Thu Feb 15 20:59:48 EST 2007
Jerry,
Try the existing burners first (Reil, Porter, etc.). The work *really*
well, and I don't think they will work as well if you put screen in
them. There is no problem in these burners with the flame climbing the
tube, the flame is controlled by the flare at the business end.
Steve
Jerry Smith wrote:
> What kind of screen was it and if it isn't hardware
> store stuff, we can I buy some?
>
> Jerry
>
> --- Grover Richardson
> <grover.richardson at gtri.gatech.edu> wrote:
>
>
>>The screen performs two purposes. One is to mix the
>>gas, the other is a
>>fire block. A third thing that is generally
>>unnoticed is that the screen
>>also keeps infra red from getting back to the
>>orifice. I have a plumbing
>>pipe version of a burner and I ran it a few times
>>without a twist of shim
>>stock inside it for a mixer. There was enough infra
>>red in the forge to
>>ignite the flame at the orifice. A fun time was had
>>by all until the burner
>>was turned off<G>.
>>
>>-----Original Message-----
>>From: theforge-bounces at mailman.qth.net
>>[mailto:theforge-bounces at mailman.qth.net] On Behalf
>>Of Bruce Freeman
>>Sent: Thursday, February 15, 2007 2:26 PM
>>To: theforge at mailman.qth.net
>>Subject: Re: [TheForge] Traveling Gas
>>
>>Lynn,
>>I don't understand your question. Who says it would
>>not be a good idea?
>>Bruce
>>NJ
>>
>>
>>>>>langfarm at together.net 2/15/2007 2:18 PM >>>
>>
>>Hello
>>
>>Why would it not be a good idea to add a screen, as
>>metal window screen
>>, between the mixing chamber and the burn area? This
>>is used in the
>>boating world to keep flames from going back down
>>the fill pipe..
>>
>>
>>
>>Lynn
>>
>>
>>
>>
>>
>>
>>
>>
>>
>>Happens all the time. The mixture just has to move
>>faster than the
>>flame front so the fire doesn't travel back up into
>>the mixing chamber.
>>
>>
>>
>>CraigS
>>
>>
>>
>>_______________________________________________
>>Manage membership or unsubscribe at:
>>http://mailman.qth.net/mailman/listinfo/theforge
>>theforge mail list group photo site is
>>http://www.photoaccess.com
>>Login: blacksmithblacksmith at hotmail.com
>>password: anvil
>>___________
>>
>>
>>
>>_______________________________________________
>>Manage membership or unsubscribe at:
>>http://mailman.qth.net/mailman/listinfo/theforge
>>theforge mail list group photo site is
>>http://www.photoaccess.com
>>Login: blacksmithblacksmith at hotmail.com
>>password: anvil
>>___________
>>
>>
>>_______________________________________________
>>Manage membership or unsubscribe at:
>>http://mailman.qth.net/mailman/listinfo/theforge
>>theforge mail list group photo site is
>>http://www.photoaccess.com
>>Login: blacksmithblacksmith at hotmail.com
>>password: anvil
>>___________
>>
>>
>>
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
More information about the TheForge
mailing list