I use a lot of those around the shop as well as plain
carbon steel ones. They all welded for me. Burn the
paint off then hammer with flux after heating.

Jerry

--- "Washington, Aubrey O." <awashington at ou.edu>
wrote:

> Jerry,
> 
> I have a bunch of old hack saw blades, but I think
> most are bimetal.  Do you think bimetal blades will
> work?
> 
> Aubrey
> 
> ________________________________________
> From: theforge-bounces at mailman.qth.net
> [theforge-bounces at mailman.qth.net] On Behalf Of
> Jerry Smith [jerry_smith at anvilsandinkstudios.com]
> Sent: Thursday, December 13, 2007 12:53 PM
> To: The Forge
> Subject: [TheForge] Hacksaw Blades was Banding steel
> 
> The reason I asked about the banding steel, is that
> a
> few years ago I made a rough twist Damascus out of
> hacksaw blades. It made a pretty knife that I saw it
> was what you could get out of Medieval Times.
> 
> I made the billet, then took two pieces of 1/4"
> steel
> rod, twisted them into a caduceus like pattern. Then
> I
> flattened them out and forged them on to the knife
> blade. This was more for show than using, but it
> made
> a pretty pattern.
> 
> Jerry
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
> 
> 
> 



More information about the TheForge mailing list