Don,
I hate to offer such a low tech solution, but a star drill may be the answer
that you need. Last time I needed a small one I found it at Sears. I tapped and
turned and tapped and turned and poured the water and tapped more. Eventually I
had a hole where I wanted it. May work for you.
Quoting PlumDon at aol.com:

> My Main Line customer wants a boot scraper in the shape of a canary  (Her
> small mansion is "Canary Cottage"). No problem making the  scraper. She also
> gave
> me one of her driveway Belgian blocks to mount it in. My  pretty good
> Milwaukee hammer drill doesn't even dent this stone. I dont know  what they
> are
> typically cut from but it is REALLY hard.;
>
> Anyone know of a way to drill it or should I just try to convince her I  need
> to use another stone.
>
> Kindest thanks for any help.
>
> Don Plummer
>
>
>
> **************************************See AOL's top rated recipes
> (http://food.aol.com/top-rated-recipes?NCID=aoltop00030000000004)
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
>
>
>


Tod Estes

People do not care about how much you know
until they know about how much you care.


More information about the TheForge mailing list