Howdy Aubrey.  I've decided that I'm going to have to split them up, but I 
think I'll try and sell the 2 big guys first(100 and 250, it's really, 
really BIG), then the Fifty and then the 25.  The 25 is a fantastic machine. 
I sent a lot of the moving parts to Sid, and he did a wonderful job of 
getting them in tolerance, and that 25 can purr, or growl.  Freshly painted 
as if that mattered (some like them left in their barn clothing)and a new 1 
HP motor.  The 50 didn't need a thing done to it, but it did get a new motor 
(1.5 HP).  Anyway, I'll try to work up some prices and get them on the right 
pages, etc.
Robert

----- Original Message ----- 
From: "Washington, Aubrey O." <awashington at ou.edu>
To: "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Thursday, December 06, 2007 4:29 PM
Subject: RE: [TheForge] Trip Hammer Report (Longish)


Robert,

Are you still trying to sell all 4 LGs as a package?  I hope you find a 
suitable buyer who appreciates the set.

Aubrey

________________________________________
From: theforge-bounces at mailman.qth.net [theforge-bounces at mailman.qth.net] On 
Behalf Of robert hensarling [rhrocker at hilconet.com]
Sent: Thursday, December 06, 2007 4:03 PM
To: Sponsored by ABANA
Subject: Re: [TheForge] Trip Hammer Report (Longish)

Aubrey, I used Dave's video to tune up my 100 Little Giant.  I also added a
spring guard and a brake, at his suggestion.  He and I emailed back and
forth for several months during my renovation, he was a fantastic person,
and a gentleman.  I just don't understand why good people like that have to
leave us, and others, that shouldn't be allowed out of their cell, go free
to kill again.
Sorry, anyway, the tape helped me a LOT!  My 100 pounder can close a match
box now (ok, ok, every once in a while it really closes the match box, big
time.
Watch it several times, and use your rerun a lot to back up and see short
segments again.  Pay attention to what's happening in the background also,
lots of info there to be had.  The lead-in part of the tape, as well as the
lead-out part, show many neat things he does with his hammer.  He has a 2nd
tape out also, and he goes in to detail on making jigs, and tooling for his
hammer.  It's as valuable as the first tape.
It makes me a little sad to sell my hammers, but I had a good time with
those Little Giants.  My shop is only big enough for my air hammer now, and
the 25, 50, 100, and 250 LG's must go.  I'll be advertising them in the
classifieds in a little bit.
Get the tapes!!  or cd's.  Very valuable!
Robert Hensarling
4326 E. Main
Uvalde, Texas 78801
www.mesquiterocker.com
www.hensarlingknives.com
Uvalde, Texas
----- Original Message -----
From: "Washington, Aubrey O." <awashington at ou.edu>
To: "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Thursday, December 06, 2007 3:52 PM
Subject: [TheForge] Trip Hammer Report (Longish)


Greetings All,

This is an up-date on my attempts to get my new/old Mayer Bros. 25# trip
hammer up and running.  My daughter's house burned down on Thanksgiving day
(night), so that took me away from the hammer for awhile.  But, in the
meantime I've corresponded a little with Sid.  The main problem is that
timing is off with the  bang-tap-miss thing going on.  Sid says there are
about 200 things that can cause this, but the first thing to consider is
that the spring is either too loose or too tight (most often too tight, in
his experience).  So, last night I finally got back into the shop to monkey
with it some.

I started by loosening the spring in increments, but that seemed to make it
worse.  Next I tried tightening it.  It seemed to get a little better, but
still not right.  Then it occurred to me that the fact that the hammer was
walking, hopping, and rocking all around the shop while I ran it might be
contributing to the problem.  (Duh.)  I'm not ready to bolt it to the floor
of the shop, so I made a wooden platform 2' X 4' X 3" to bolt it to.  The
next problem was how to lift the hammer onto the platform since I don't have
any kind of hoist in my shop that will lift 900 pounds (with the motor
removed).  What finally worked (barely) was a lift boom on the 3-pt hitch of
my 1948 Ferguson tractor.  That was the absolute limit of my tractor's
lifting capacity at the 6 foot level (though I could probably lift more
closer to the ground).  By the time I got the hammer wrestled onto the
platform, it was cold, dark, and dinner time.  So, it will be this weekend
before I can get it bolted down and try again on the adjustments.

I have ordered Dave Manzer's DVD on trip hammers from Anvilfire, but it has
not arrived yet.  I can't wait!  In the meantime, I'll entertain all
speculation about how to fix my problems.  (No, not those problems, Frosty!)

Aubrey
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________




_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________






More information about the TheForge mailing list