[TheForge] Back from the Pennsic Wars
Jerry Frost
akfrosty at mtaonline.net
Wed Aug 22 01:18:05 EDT 2007
Dann:
Do you have a picture of the coil muller? URL? Etc.?
Frosty
-------------------------------
If it ain't forged
it ain't real.
Wrought iron is.
The FrostWorks
Meadow Lakes, AK.
http://www.artmetalradio.com/
From: <dan at irontreeworks.com>
> It's not my design. It's a period one from a book. I
> don't know which one. I
> could ask if you want. I didn't make it. It was made
> by a friend, Tim Park.
> Feel free to copy it. I'll tell him you liked it.
>
> Danr
>