[TheForge] Burner types was Fixing my forge
GHS
GHS at execpc.com
Fri Aug 10 16:30:28 EDT 2007
Jerry Frost wrote:
>
> There is wiggle room in the bore length but not a lot, making it much
> longer or shorter will inhibit induction. If you have to make the tube
> longer increase the diameter about 25% every time you double the
> length. For example a 1" bore 8 or 9" long is fine, make it longer and
> increase it to 1 1/4" dia till you hit 17 - 18" then increase it
> again. I have no idea how long you can do this but am sure it isn't
> forever. Probably only a couple step increases. If you can taper the
> entire length of the tube you can make one quite long and only
> increase induction.
>
Jerry, if you add one of Zoellers flares to this does it count as just
,more bore length, not count at all,1/2 ????
Mike Graf
--
Please visit us at http://www.gaudeteforge.com/
More information about the TheForge