Terry:
What are you using for grog and temp is this refractory
recipe good for?
Frosty
-------------------------------
If it ain't forged
it ain't real.
Wrought iron is.
The FrostWorks
Meadow Lakes, AK.
http://www.artmetalradio.com/
From: "terry l. ridder" <terrylr at blauedonau.com>
> hello;
>
>
> the home brewed lining recipe from the book is;
> 4 gallons of silica sand
> 4 gallons of grog
> 4 gallons of fire clay
> 3 quarts of borax powder
>
> i have mixed up;
> 10 gallons of silica sand
> 10 gallons of grog
> 10 gallons of fire clay
> 8 quarts of borax powder
>
>
> --
> terry l. ridder ><>