[TheForge] Heat treat for Titanium
Bob Ehrenberger
eforge at centurytel.net
Mon Sep 4 23:24:01 EDT 2006
I really have no idea what variety of titanium I have. In this area most
high tech materials originate at the McDonnel-Douglas/Boweing scrap bin in
St. Louis. The piece I started with was a sheet 3/16 thick by 6" by 12"
maybe part of an armor plating system. Or it may be a drop left over after
the primary piece was cut out. You really never know with scrap.
I did try a better piece of flint today and got better results.
I will try the process that Dave recomended and report back if it helps.
The main reason I hadn't tried quenching it was I really had no idea how
titanium would react. It appears that it is at least feasable to water
quench and then temper, I'll give it a shot.
Robert Ehrenberger
Shelbyville, Mo.