[TheForge] Any recommendations on cutoff saws? Brands, etc?

Ron Childers munlaw2 at hcsmail.com
Fri Sep 1 14:51:59 EDT 2006


That sounds like a wood saw blade unless the cutters are in line and
separated by 1/4" holes......If it looks like a wood cutting blade it
probably is, and that could get u killed.

Ron C

-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Michael
Sent: Friday, September 01, 2006 2:05 PM
To: 'Sponsored by ABANA'
Subject: RE: [TheForge] Any recommendations on cutoff saws? Brands, etc?

Frosty,
What is the blade diameter and RPM?
Mikey

-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Jerry Frost
Sent: Friday, September 01, 2006 10:13 AM
To: Sponsored by ABANA
Subject: Re: [TheForge] Any recommendations on cutoff saws? Brands, etc?

The blade has big carbide teeth and looks like a big 
skill saw blade. It's a Jet.

Frosty
-------------------------------
If it ain't forged
it ain't real.
Wrought iron is.
The FrostWorks

Meadow Lakes, AK.

http://www.artmetalradio.com/

From: "Michael" <michael.a.porter at comcast.net>



> Frosty,
> Dry-cut is a term used for some kinds of diamond 
> blades and also for special
> reduced speed soft carbide tipped (boron added) 
> cut-off saws. By reduced
> speed, I mean that a fourteen inch blade diameter 
> would spin at about 1300
> RPM (ex. Porter Cable's 1410P 14" Dry Cut Saw). The 
> teeth also have a
> different geometry (no rake). They cut like a miracle 
> as long as you don't
> break the rules, but they are very unforgiving if you 
> do. The moose you use
> at work sounds very much like a Trennager 
> air-friction steel blade cut-off
> saw (is the tooth geometry like crooked fingers with 
> rounded ends?). Used
> one daily for months back in the early sixties. It 
> was a real monster.
> Mikey
>

_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________




_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________





More information about the TheForge mailing list