Mike Linn wrote:
>
> Heat them to critical, and water quench them, then all you have to do 
> is drop it on the floor to watch it shatter...
>
Yep - I once made the mistake of quenching a piece of unknown junkyard 
steel in superquench, that didn't even wait to be dropped to shatter.

--Justin Fisher