The corn meal was an ingredient, I think ANCO the windshield wiper people
used to make something similar!
Rowland of Roseburg, OR 97470
I love The Science Channel
My Hero's are Burt Rutan & Paul McCready
----- Original Message -----
From: "Bruce Freeman" <FREEMAB at pt.fdah.com>
To: <theforge at mailman.qth.net>
Sent: Tuesday, November 14, 2006 7:48 AM
Subject: Re: [TheForge] Lowes has lye
> OUT of corn meal, or with corn meal in it?
> Bruce
> NJ
>
>>>> rsmuck at hughes.net 11/13/2006 1:47 PM >>>
> Bruce, I used to have a customer who was a chemical company, they made
> up
> hand soap out of Corn meal, I loved it, wish I knew where to get some!
> Rowland of Roseburg, OR 97470
> I love The Science Channel
> My Hero's are Burt Rutan & Paul McCready
> ----- Original Message -----
> From: "Bruce Freeman" <FREEMAB at pt.fdah.com>
> To: <theforge at mailman.qth.net>
> Sent: Monday, November 13, 2006 6:37 AM
> Subject: Re: [TheForge] Lowes has lye
>
>
>> Soapmaking. Or will be. My range oven conked out over the weekend,
> and
>> there went my free time.
>>
>> I made a crude batch of lye soap about six months ago and have been
>> very impressed with it. It's very effective and long-lasting. It
>> doesn't sop up water and decay into mush, but forms a good lather on
> the
>> hands. It's not particularly harsh. And it has no stinkin'
> perfume!
>>
>> I've nowhere near run out of the stuff, but it's ugly yellow stuff
> from
>> cooking grease. I want to make some that looks nicer in the bath by
>> starting with white grease. I may experiment with other oils and
> fats
>> too.
>>
>> Bruce
>> NJ
>>
>>>>> wjec at verizon.net 11/11/2006 6:34 PM >>>
>> What are you using this for Bruce?
>>
>> ----- Original Message -----
>> From: "Bruce Freeman" <freemab222 at yahoo.com>
>> To: "theforge" <theforge at mailman.qth.net>
>> Sent: Saturday, November 11, 2006 2:57 PM
>> Subject: [TheForge] Lowes has lye
>>
>>
>>> Found lye sold retail locally at Lowes home centers.
>>> Look for Roebic Crystal Drain Opener in the plumbing
>>> dept. Tall, white plastic jar with mostly yellow
>>> label. Claims to be 100% sodium hydroxide (lye) and
>>> appears to be so.
>>> Bruce
>>> NJ
>>>
>>>
>>>
>>>
>>
> ____________________________________________________________________________________
>>> Do you Yahoo!?
>>> Everyone is raving about the all-new Yahoo! Mail beta.
>>> http://new.mail.yahoo.com
>>> _______________________________________________
>>> Manage membership or unsubscribe at:
>>> http://mailman.qth.net/mailman/listinfo/theforge
>>> theforge mail list group photo site is
>>> http://www.photoaccess.com
>>> Login: blacksmithblacksmith at hotmail.com
>>> password: anvil
>>> ___________
>>>
>>>
>>>
>>
>>
>> _______________________________________________
>> Manage membership or unsubscribe at:
>> http://mailman.qth.net/mailman/listinfo/theforge
>> theforge mail list group photo site is
>> http://www.photoaccess.com
>> Login: blacksmithblacksmith at hotmail.com
>> password: anvil
>> ___________
>>
>>
>> _______________________________________________
>> Manage membership or unsubscribe at:
>> http://mailman.qth.net/mailman/listinfo/theforge
>> theforge mail list group photo site is
>> http://www.photoaccess.com
>> Login: blacksmithblacksmith at hotmail.com
>> password: anvil
>> ___________
>>
>>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
More information about the TheForge
mailing list