[TheForge] Gotta froze-up Champion blower
Bruce Freeman
FREEMAB at pt.fdah.com
Mon Nov 13 14:53:27 EST 2006
A friend of mine soaks stuck things in kerosene, sometimes spiked with
oil.
(If it's all steel and rusted, you're better off soaking off the rust
in weak acid.)
Bruce
NJ
>>> rfertner at cox.net 11/13/2006 2:06 PM >>>
I have used PB blaster from the auto parts store. I spray and saturate
the blower several times over a few days until things start coming
loose.
Rob
---- Grover Richardson <grover.richardson at gtri.gatech.edu> wrote:
> I broke loose an old 32 Buick by squirting in WD-40, putting it in
second
> gear, and rocking it back and forth. Repeat daily for about a week.
Works.
>
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net
> [mailto:theforge-bounces at mailman.qth.net] On Behalf Of Ron Childers
> Sent: Monday, November 13, 2006 8:32 AM
> To: 'Sponsored by ABANA'
> Subject: RE: [TheForge] Gotta froze-up Champion blower
>
> Champion 400? #1: Don't try to pry or wedge the brass gear. Also, the
fan
> blades are riveted to a cast blade mount- don't beat on them. Try
cleaning
> with mineral spirits or other solvent. Loosen the rear bearing keeper
and
> try gently tapping the crank and working back and forth. The bearings
are
> all different. The bearings in the rear are 1/4" balls, available @
Miller
> Bearings in sacks of 100 for about $10. There are some bronze
bushings and
> some caged bearings. I'm told the bearings out of an old Schwin
bicycle will
> work for some of the bearings. I don't have the patience to mess with
it. I
> think my 400 would make a good target for my Ruger Redhawk 44
magnum.....
>
> Ron Childers
>
>
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net
> [mailto:theforge-bounces at mailman.qth.net] On Behalf Of Lou
Polsinelli
> Sent: Monday, November 13, 2006 7:36 AM
> To: theforge at mailman.qth.net
> Subject: [TheForge] Gotta froze-up Champion blower
>
> Hi folks:
> I've acquired a champion that's froze up. Assuming it's just gunked
up
> inside, is there an alternative to taking it apart . If I do have to
> take it apart, any hints as to what to do or what not to do?
>
> Thanks in advance for any advice you can give me.
>
> --Lou P.
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge
mailing list