[TheForge] ranite hardfacing rods
Washington, Aubrey O.
awashington at ou.edu
Wed May 24 09:51:00 EDT 2006
That would sure be easier than trying to wrestle the thing in and out of the forge. Too bad I don't have a rosebud.
________________________________
From: theforge-bounces at mailman.qth.net on behalf of Darrell
Sent: Tue 5/23/2006 6:23 PM
To: Sponsored by ABANA
Subject: Re: [TheForge] ranite hardfacing rods
You should be able to use a large rosebud and hammer shape the horn.
Darrell
----- Original Message -----
From: "Washington, Aubrey O." <awashington at ou.edu>
To: "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Tuesday, May 23, 2006 2:51 PM
Subject: RE: [TheForge] ranite hardfacing rods
I suppose that would be an option, but I don't think I'll do any welding on
this anvil.
________________________________
From: theforge-bounces at mailman.qth.net on behalf of Dan Tull
Sent: Tue 5/23/2006 4:47 PM
To: Sponsored by ABANA
Subject: Re: [TheForge] ranite hardfacing rods
I have miged a bolt to the wrought then built up around to a needle point.
----- Original Message -----
From: "Washington, Aubrey O." <awashington at ou.edu>
To: "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Tuesday, May 23, 2006 3:52 PM
Subject: RE: [TheForge] ranite hardfacing rods
I just picked up a 105# Mouse Hole that is in reasonable shape for its age.
But, the tip of the horn is mushroomed a bit and there are some rather deep
cuts (~1/8") on the horn. I can work around the cuts, but my question is
about the mushroomed tip. Has any of you ever tried reforging the wrought
iron tip of a horn? Is this a practical thing to try? What are the
hazards? I wouldn't be messing with the steel face at all (which is in
reasonably good shape).
The really odd thing about this anvil is that the face is not parallel to
the base so that when the anvil is sitting on a level surface, the horn-end
of the face is a good 1/4 to 1/2 inch lower than the heal. It seems to have
been forged that was since there is no obvious abuse of the anvil that would
have caused this.
Aubrey
Rock Creek Forge
Norman, OK
________________________________
From: theforge-bounces at mailman.qth.net on behalf of Ron Childers
Sent: Tue 5/23/2006 1:49 PM
To: 'Sponsored by ABANA'
Subject: RE: [TheForge] ranite hardfacing rods
That's why I made a 3/8" lilt for the hardy hole on my Hay Budden
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Dan Tull
Sent: Tuesday, May 23, 2006 2:13 PM
To: Sponsored by ABANA
Subject: Re: [TheForge] ranite hardfacing rods
I sold a 180# P/W and kept a 179# P/W because the 180 was too flat.
It was easier to straighten stock on the sway.
----- Original Message -----
From: <schade at acegroup.cc>
To: "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Tuesday, May 23, 2006 12:13 PM
Subject: Re: [TheForge] ranite hardfacing rods
>
> On May 23, 2006, at 10:44 AM, Luke Thomson wrote:
>
>> After reading your reviews I am doubting that my anvil needs to be
>> refaced, just repaired. I plan on getting some sticks or maybe wire if
>> I can today. I've posted some pictures on photoaccess under tools and
>> tooling ( it wouldn't let me create a new album...) My pictures show
>> the gashes but I was unable to show the sway very well.
>> Does anyone know any reason why not to run tig beads across the anvil?
>> Seems like that would both reduce the amount of grinding and, more
>> importantly, give me some more practice with TIG.
>> Thanks for all your help,
>> Luke
>>
>
>
>
> couldn't find your pictures. Some sway isn't really that big a problem.
> My advice would be to get something you can use as an anvil. track,
> large object etc. After working a while you will know better what your
> requirements are. don't get bogged down in having a perfect anvil.
>
> Bob
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
--------------------------------------------------------------------------------
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
--------------------------------------------------------------------------------
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge