[TheForge] Another hollow sphere idea
Jerry Frost
frosty at customcpu.com
Tue Mar 21 01:10:48 EST 2006
Hmmmm.
I can't say one way or another except to compare to a standard propane
forge, reverberatory furnace, where the steel isn't heated primarily by the
direct flame but by IR from the furnace walls.
I don't know enough to discuss it intelligently however I can find out easy
enough. Once I get one built, I'll get it up to heat and time a bar to heat,
fire on and fire off.
It's a good point Bruce and could save a bunch of fooling around on a false
premise.
So, my first chips will be palm rounded cubes.
Frosty
-------------------------------
If it ain't forged
it ain't real.
Wrought iron is.
The FrostWorks
Meadow Lakes, AK.
http://www.artmetalradio.com/
From: "Bruce Freeman" <FREEMAB at pt.fdah.com>
Keep us posted on your progress. I'd be working on a chip forge too, if I
had the time...
Here's the reason I think that heat transfer from the chips may prove less
important than from the flames:
I work with chromatography, which often involves heating a "column" (think
"tube"), either empty or packed, to aid in the motions of chemical compounds
down the column. Formerly, the common wisdom was that you got the column up
to temperature and that was that. When you injected a cooler material (the
sample) it was assumed that it was heated by the hot tube and/or packing.
Then someone did the math. Pretty simple, really, but if you don't ask the
question, you don't get the answer.
It turns out that the heat for warming the sample comes from the fluid
entering the column, NOT from the tube or packing. By analogy, I strongly
suspect that the chips in a chip forge act as little more than support for
the steel being heated and as INSULATION against cooling. I have not proven
this, nor do I intend to any time soon. I toss it out as food for thought.
If this is the case, then we want "chips" that are easy to work around, that
don't impede the flames, and that don't take forever to heat up. Preferably
they should be penetrated by the flames (i.e., should be hollow).
Bruce
NJ
>>> frosty at customcpu.com 3/17/2006 4:47:38 PM >>>
This sounds workable, maybe even easy, definitely worth a try.
Heating the metal is largely transfer from the chips to the steel but the
burning gas will be carrying part of the load as well. So, if this works
easily enough then it'll be a matter to determine how thick to make the
shell.
If I have time this weekend I'm going to try ramming up a test forge. I'll
be using a fire clay, sand, cement refractory for the tests. Once I get a
workable unit I'll use a high end refractory, either alumina or high
phosphate rammable. (I already have about 60lbs of the high phosphate
rammable)
For the tests I'll make the rounded off cubes for chips and again use a high
end refractory once I get a working shape/size/etc.
I'll also make a small quantity of barrel and life saver shapes starting
with 3/4" x 3/4" and tweeking from there.
Don't know how far I'll get this weekend, we have a vet clinic and a number
of critters to take, a wood stove to install and a barn to clean. I might
not get farther than the forms but I have everything on hand so who knows.
Frosty
-------------------------------
If it ain't forged
it ain't real.
Wrought iron is.
The FrostWorks
Meadow Lakes, AK.
http://www.artmetalradio.com/
From: "Bruce Freeman" <FREEMAB at pt.fdah.com>
I just caught up with the postings.
I liked the idea of slip-casting hollow spheres, but agree it would be very
slow.
How about a modification to my wooden bead idea:
String wooden beads or styrofoam spheres (~1/2" dia) on a 1/4" dowel. Dip
the dowel in a castable refractory and let it set. (Repeat if necessary,
but preferably have a mix of the appropriate viscosity to do it in one dip.)
Fire "slow" to dry the refractory, then to full heat to fuse it. By this
time the dowel will have burned off, so work over an appropriate material so
the whole mess doesn't fuse together. This should work fairly quickly, once
the bugs are worked out.
And to clarify WHY hollow spheres may be desirable:
1) Spheres won't pack tightly - hence burning gases will pass through
easily, AND it should be easy to insert the object to be heated.
2) Spheres are relatively strong, so won't easily crush.
3) Being hollow and perforated, the hot gases will (to some extent) pass
through them.
4) Being relatively (?) thin shells, there is no issue of heat "from the
center" taking long to get to the surface.
The presumption here is that we want the burning gases to do the heating,
and not to be heating using heat stored in the chips.
Bruce
NJ
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge
mailing list