[TheForge] burners and other addictions
Mike Porter
michael.a.porter at comcast.net
Sat Mar 18 20:51:09 EST 2006
Frosty,
OK, I should have said weld well enough to be certified. It isn't just the
intense heat available from an oxyacetylene flame that's needed, but also
the excess carbon in the flame, for acceptable steel welds. Mind you, if
someone can come up with a way around the problem, I would be the first to
applaud it. I may do some experiments mixing carbon into flux this summer
just to see if the "wall" can be breached somehow, as I would dearly love to
move acetylene clear out of the must have category.
Mikey
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Jerry Frost
Sent: Friday, March 17, 2006 5:30 PM
To: Sponsored by ABANA
Subject: Re: [TheForge] burners and other addictions
I don't recall anything about investors but I didn't spend a lot of time on
the site. I wouldn't be surprised if it were the same folk though.
My All States oxy/propane torch welds. Not terribly well admitedly, the
velocity of the flame is so high it blows the puddle around too much, but it
does weld. I have a lot better alternatives so don't weld with it.
Still.
Frosty
-------------------------------
If it ain't forged
it ain't real.
Wrought iron is.
The FrostWorks
Meadow Lakes, AK.
http://www.artmetalradio.com/
From: "Mike Porter" <michael.a.porter at comcast.net>
> Frosty,
> This torch is beginning to sound familiar. There was such a torch being
> advertised on some UK site several years ago. As I recall, they were
> looking for 'investors' (which in my view would be spelled somewhat
> differently, beginning with an "s" as well as ending with one). And, you
> should know that the only gas that will weld steel is acetylene, because
> of all the free carbon it has available.
> Mikey
>
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge