>I haven't seen the plans but if I was making a firepot for a coal forge 
> I would make the air inlet higher that the lowest point of the pot so 
> that clinker wouldn't block the flow of air. Clinker breakers *fix* a 
> problem that doesn't have to be there.
> 
> Bob
> ___________
> 
> 
> 
> 
> On Jun 28, 2006, at 10:54 PM, Fred Zickrick wrote:
> 
>> I'm using an old tractor rim that I found in a junk pile (nostalgia??) 
>> on our farm as the container for my "portable forge".  It's about 20" 
>> inside diameter.
>>
>> I've already used Bob Patrick's plans for the all-steel firebox to 
>> build a firepot modified for the constraints of my rim.  It's 8x7 at 
>> the top sloping down to 5x5 at the bottom, is 3.75 deep and is made of 
>> 3/8ths mild steel.
>>
>> I have an old castiron tuyere that has an inside diameter of just 
>> under 4".  I was going to make a grate at the bottom to fit over the 
>> tuyere out of the 3/8ths plate with slots cut in it.  I'd planned to 
>> put a fair amount of opening in the grate.
>>
>> I felt pretty good about the dimensions until I read some info at 
>> Lytton Creek and now I feel I may have made the box and grate too big. 
>>    Also, LC seems to imply that I should have made the whole thing out 
>> of at least 1/2" plate.
>>
>> What do y'all think of the dimensions?  This is not supposed to be my 
>> only forge just something to get started with and use at hammer-ins 
>> but y'all know how that goes!
>>
>> Thank you,
>> Fred Zickrick, fredz72 at cableone.net
>> _______________________________________________
>> Manage membership or unsubscribe at:
>> http://mailman.qth.net/mailman/listinfo/theforge
>> theforge mail list group photo site is
>> http://www.photoaccess.com
>> Login:  blacksmithblacksmith at hotmail.com
>> password:  anvil
>> ___________
>>
>>
>>
> 
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
> 
>


More information about the TheForge mailing list