On a set of little giant dies I've repaired chips by tig welding the
void using an uncoiled spring (~1/8" diam wire) as filler material.
I'd guess most springs are 5160 -ish in composition. I've had
surprisingly little cracking of these repairs.
Cameron Stoker
cameron at stoker.net
"May you run like a vicuña!"